ABchimie 80K UV LED High Viscosity Resin

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ABchimie 80K UV LED High Viscosity Resin

Main features

  • Soft, flexible resin
  • Excellent adhesion
  • UL 94 V‑0 flammability rating

Product Description

ABchimie 80K UV LED is a soft, one‑component resin optimized for UV LED curing, providing rapid, energy‑efficient polymerization with low heat generation. It is designed for local protection and mechanical reinforcement, especially for tall or vibration‑sensitive components.

The resin supports high‑thickness applications up to 5 mm, offering robust humidity and thermal resistance. With strong adhesion to numerous substrates and no VOC, ABchimie 80K UV LED enables clean and efficient processing in modern electronic manufacturing environments.

Product Key Features

  • Soft, flexible resin for shock and vibration damping
  • Excellent adhesion on PCBs, plastics, and other substrates
  • High‑speed process suitable for modern LED‑equipped production lines
  • One‑component, ready‑to‑use formulation
  • UL 94 V‑0 flammability rating qualified (QMJU2‑E308681)

Applications

  • Local encapsulation using UV LED curing systems
Product Family

234395

Résine ABchimie 80K UV LED 01K
1. Select Package Type

Loading pricing…

Product availability
EU Shipping in 8 weeks
Packaging
Unit of measure Can
Net weight 1 kg
Gross weight 1.1 kg
Dimensions 9 x 9 x 21 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Transparent liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.1
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
80000 mPa.s
Mechanical Properties
Durometer (Shore D)
15
Thermal Properties
Coefficient of Thermal Expansion (CTE), α1
CTE α1 (alpha 1) is the slope of the Coefficient of thermal expansion in a temperature range below the Glass transition temperature (Tg). It explains how much a material will expand until it reaches Tg.
50 ppm/°C
Coefficient of Thermal Expansion (CTE), α2
CTE α2 (alpha 2) is the slope of the Coefficient of thermal expansion in a temperature range above the Glass transition temperature (Tg). It explains the extent to which a material will expand after it passes Tg.
150 ppm/°C
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
-19 °C
Electrical Properties
Breakdown Voltage
Breakdown voltage is the minimum voltage necessary to force an insulator to conduct some amount of electricity. It is the point at which a material ceases to be an insulator and becomes a resistor that  conducts electricity at some proportion of the total current.  After dielectric breakdown, the material may or may not behave as an insulator any more because of the molecular structure alteration. The current flow tend to create a localised puncture that totally alters the dielectric properties of the material. This electrical property is thickness dependent and is the maximum amount of voltage that a dielectric material can withstand before breaking down. The breakdown voltage is calculated by multiplying the dielectric strength of the material times the thickness of the film.
1500 V
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
60 kV/mm

Additional Information

Curing Profile

Recommended settings for the best properties of the resin ABchimie80K UV LED (LED lamp 395 nm):

  • Minimum UVA2 dose : 3000mJ/cm2 (to a 1mm-thickness)

The UVA dose is a minimum dose recommended. The intensity depends on the lamp power and the lampe distance.

UVA dose may be increased by a longer exposure time. A higher dose of UV or an overexposure will not damaged the product. However a lower UVA dose can have a detrimental effect on product final properties therefore it is very important to ensure minimum recommended UVA dose is met with your curing system.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers