ABchimie 9005UV Glue

Harmonization Code : 3906909090 | Acrylic polymers in primary form Others>Others

ABchimie 9005UV Glue

Main features

  • One-component
  • Fast UV Curing
  • Glass to multiple substrate adhesion

Product Description

ABChimie® 9005UV Glue is a clear glue designed for the bonding of glass to multiple substrates, including glass, metals, and plastics. It is optically clear and doesn't experience yellowing. ABChimmie 9005UV Glue is ideal for applications requiring adhesion to glass and other substrates and optical transparency. 

ABChimie 9005UV Glue is a urethane acrylate-based product with excellent adhesion to various substrates, especially glass. It cures rapidly under UV light, has zero VOCs, and can be applied to high-speed manufacturing processes to increase productivity. ABChimmie 9005UV Glue is in full compliance with REACH and RoHS regulations.

Product Key Features

  • Transparent urethane acrylate glue
  • No yellowing
  • Allows for thick, controlled application 
  • Fast UV cure (mercury lamp) for high-speed processing
  • Solvent-free formulation (no VOCs)

Applications

  • Components requiring optical transparency ex. glass, lenses, transparent covers.
  • Adhesion of glass to various substrates, ex. glass to metal, glass to plastic, glass to glass etc.
  • Laminated glass to glass ex. touchscreens, sensors
  • Gap filling and bonding
  • Printed circuit assemblies. 

Product Family

234342

1kg Bulk
1. Select Package Type

Loading pricing…

Product availability
EU Shipping in 8 weeks
Packaging
Unit of measure Can
Net weight 1 kg
Gross weight 1.1 kg
Dimensions 9 x 9 x 21 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Transparent
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
55000 mPa.s
Mechanical Properties
Adhesion Strength
Adhesion is the bond strength measurement of a coating to a substrate. When an adhesive is bonded to an item or surface, numerous physical, mechanical and chemical forces come into play, which may have an effect on each other.
6962 Oz/in

Additional Information

Frequently Asked Questions About ABChimie® 9005 UV

What are typical applications for ABChimie® 9005 UV?

ABChimie® 9005 UV is a UV-curable glue designed for the bonding and protection of printed circuit board assemblies (PCBs) and electronic components in demanding manufacturing environments, including:

  • Automotive electronics (e.g., control units, sensors)

  • Industrial automation (e.g., motor drives, PLCs)

  • Consumer electronics (e.g., smart devices, wearables)

  • Other high-reliability electronic assemblies

Why choose ABChimie® 9005 UV?

ABChimie® 9005 UV delivers rapid UV curing, excellent electrical insulation, is colorless, and has strong adhesion to various substrates. It supports high-throughput manufacturing while providing durable protection for sensitive components.

What is the shelf life of ABChimie® 9005 UV?

ABChimie® 9005 UV has a shelf life of 12 months when stored at 5–30°C in tightly sealed, opaque containers. The product must be sealed away from excessive heat (>40°C). Before use, allow the product to equilibrate for 24 hours at 18–32°C for optimal performance. Due to settling, glue should be mixed before use.

What happens after the shelf life?

Using ABChimie® 9005 UV past its shelf life may alter viscosity, affecting uniformity and application performance. Always use an in-date product for reliable results.

What is the recommended curing method for ABChimie® 9005 UV?

ABChimie® 9005 UV is UV-curable and should be cured with a mercury lamp. The minimum UVA dose is 500 mJ/cm² for a 100 μm thickness. The LED-curable version is ABChimie® 9005 UV LED. Higher UVA doses do not negatively affect final properties.

What is the maximum thickness for ABChimie® 9005 UV?

ABChimie® 9005 UV can be applied up to 4mm due to its thixotropic properties, allowing high-thickness deposits without sagging.

What safety precautions should I take?

Use ABChimie® 9005 UV in a well-ventilated area, avoid skin and eye contact, and follow all Safety Data Sheet (SDS) guidelines. Keep away from open flames and sparks.

Can I adjust viscosity?

ABChimie® 9005 UV can be customized for variable viscosities. Contact our team for guidance.

Learn More About ABChimie® 9005 UV


ABChimie® 9005 UV is a proven solution for engineers seeking fast, reliable protection of electronic assemblies in demanding manufacturing environments. This UV-curable glue delivers rapid curing, excellent electrical insulation, and strong environmental resistance—ideal for applications in automotive electronics, industrial automation, consumer electronics, and other high-reliability assemblies.


Main Advantages of ABChimie 9005 UV

UV Curing

ABChimie® 9005 UV cures rapidly under UV light, enabling integration into both batch and inline production. The resin forms a durable, high-performance layer that protects assemblies while supporting high-throughput manufacturing.

MECHANICAL PROTECTION

ABChimie® 9005 UV  provides excellent mechanical protection. The hardness helps resist scratches, abrasion, and minor impacts, ensuring long-term stability of encapsulated components.

no yellowing

ABChimie® 9005 UV is formulated to resist yellowing over time, maintaining clarity and optical integrity even after prolonged UV exposure. This ensures that encapsulated components or coatings remain visually clear and do not discolor, ideal for displays, optical devices, and other applications where long-term transparency is critical.

EXCELLENT ADHESION on many substrates, especially glass

ABChimie® 9005 UV bonds strongly to glass substrates, providing reliable adhesion on smooth, non-porous surfaces. This ensures durable protection for components mounted on or encapsulated against glass, making it well suited for applications such as displays, sensors, optical assemblies, and glass-based electronic modules.


How to Choose a Resin

Selecting the most suitable resin requires consideration of key factors:

  • ✔ Norms & Compliance
  • ✔ Environment / Exposure Conditions
  • ✔ Repairability
  • ✔ Electrical Performance
  • ✔ Application Method
  • ✔ Operating Temperature

Compliance You Can Trust ✅

ABChimie® 9005 UV meets stringent industry standards, ensuring reliability and regulatory adherence for OEMs and contract manufacturers:

  • REACH Compliant
  • RoHS 2011/65/EU Compliant
 

Curing Tip: ABChimie 9005 UV cures with UV rays. It is crucial to use the appropriate equipment, as well as the recommended settings, to achieve the best properties of the resin.

Emission Spectrum of Mercury Lamp

PTM6000HV-SP thermal impedance versus bondline thickness

Ref. Leistung / ref power ln % over wavelength in nm

Key Curing Properties

Lamp Type
Mercury
Emission Spectrum of Mercury Lamp
200-400 nm
Minimum UVA Dose
200 mJ/cm2 
Coating Thickness
100 μm

Typical property values shown for reference only and should not be used as specifications.




Alternative to Mercury Lamp Curing of ABChimie 9005 UV

ABChimie 9005 UV is also available in the LED - version, which cures by LED Lamp.

ABChimie 9005 UV LED [Go to 9005 UV LED Product Page↗]

  • Thixotropic resin
  • Fluorescent under UV light
  • Excellent adhesion to flexible substrates
  • Immediate curing with UV LED exposure

Best suited for: High-speed process looking to use LED light for curing

Contact Us → 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers