ABchimie 9111 UV LED Glue

Harmonization Code : 3906909090 | Acrylic polymers in primary form Others>Others

ABchimie 9111 UV LED Glue

Main features

  • One-component
  • Fast LED UV Curing
  • Adhesion to many substrates

Product Description

ABChimie® 9111UV LED Glue is a soft, clear glue designed for the bonding of multiple substrates, including glass, metals, and plastics. Its viscosity allows for controlled application with high thicknesses (up to 4mm) without sagging. These qualities make ABChimmie 9111UV LED Glue ideal for small components with high-volume production, requiring adhesion between multiple substrates and optical transparency. 

ABChimie 9111UV LED Glue is a urethane acrylate-based product with excellent adhesion to various substrates, including flexible materials such as plastics. It cures rapidly under UV LED light (395nm), has zero VOCs, and can be applied to high-speed manufacturing processes to increase productivity. ABChimmie 9111UV LED Glue is in full compliance with REACH and RoHS regulations.

Product Key Features

  • Transparent urethane acrylate glue
  • No yellowing
  • Allows for thick, controlled application 
  • Fast UV cure (LED) for high-speed processing
  • Solvent-free formulation (no VOCs)

Applications

  • Components requiring optical transparency ex. glass, lenses.
  • Adhesion to various substrates, ex. metal to glass, metal to plastic, glass to plastic, etc.
  • Rework or repair.
  • Can be used to seal plastic casings on PCBs.
  • Printed circuit assemblies. 

Product Family

234340

Colle ABchimie 9111 UV LED 01K
1. Select Package Type

Loading pricing…

Product availability
EU Shipping in 8 weeks
Packaging
Unit of measure Can
Net weight 1 kg
Gross weight 1.1 kg
Dimensions 9 x 9 x 21 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Transparent
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
10000 mPa.s
Mechanical Properties
Adhesion Strength
Adhesion is the bond strength measurement of a coating to a substrate. When an adhesive is bonded to an item or surface, numerous physical, mechanical and chemical forces come into play, which may have an effect on each other.
8354 Oz/in

Additional Information

Frequently Asked Questions About ABChimie® 9111 UV LED

What are typical applications for ABChimie® 9111 UV LED?

ABChimie® 9111 UV LED is a LED UV-curable glue designed for the bonding and protection of printed circuit board assemblies (PCBs) and electronic components in demanding manufacturing environments, including:

  • Automotive electronics (e.g., control units, sensors)

  • Industrial automation (e.g., motor drives, PLCs)

  • Consumer electronics (e.g., smart devices, wearables)

  • Other high-reliability electronic assemblies

Why choose ABChimie® 9111 UV LED?

ABChimie® 9111 UV LED delivers rapid LED UV curing, excellent electrical insulation, is colorless, and has strong adhesion to various substrates. It supports high-throughput manufacturing while providing durable protection for sensitive components.

What is the shelf life of ABChimie® 9111 UV LED?

ABChimie® 9111 UV LED has a shelf life of 12 months when stored at 5–30°C in tightly sealed, opaque containers. The product must be sealed away from excessive heat (>40°C). Before use, allow the product to equilibrate for 24 hours at 18–32°C for optimal performance. Due to settling, glue should be mixed before use.

What happens after the shelf life?

Using ABChimie® 9111 UV LED past its shelf life may alter viscosity, affecting uniformity and application performance. Always use an in-date product for reliable results.

What is the recommended curing method for ABChimie® 9111 UV LED?

ABChimie® 9111 UV LED is LED UV-curable and should be cured with a mercury lamp. The minimum UVA dose is 750 mJ/cm² for a 100 μm thickness with a 395nm LED lamp. The mercury lamp-curable version is ABChimie® 9111 UV. Higher UVA doses do not negatively affect final properties.

Recommended Settings: 
LED lamp 395 nm
Minimal Power: 150 mW/cm² (UVA2)
Distance LED light – glue: 0 to 10cm

What is the maximum thickness for ABChimie® 9111 UV LED?

ABChimie® 9111 UV LED can be applied up to 4mm due to its thixotropic properties, allowing high-thickness deposits without sagging.

What safety precautions should I take?

Use ABChimie® 9111 UV LED in a well-ventilated area, avoid skin and eye contact, and follow all Safety Data Sheet (SDS) guidelines. Keep away from open flames and sparks.

Can I adjust viscosity?

ABChimie® 9111 UV LED can be customized for variable viscosities. Contact our team for guidance.

 

Learn More About ABChimie® 9111 UV LED


ABChimie® 9111 UV LED is a proven solution for engineers seeking fast, reliable protection of electronic assemblies in demanding manufacturing environments. This LED UV-curable resin delivers rapid curing, excellent electrical insulation, and strong environmental resistance—ideal for applications in automotive electronics, industrial automation, consumer electronics, and other high-reliability assemblies.


Main Advantages of ABChimie 9111 UV LED

UV Curing

ABChimie® 9111 UV LED cures rapidly under UV light, enabling integration into both batch and inline production. The resin forms a durable, high-performance layer that protects assemblies while supporting high-throughput manufacturing.

MECHANICAL PROTECTION

ABChimie® 9111 UV LED provides excellent mechanical protection. The hardness helps resist scratches, abrasion, and minor impacts, ensuring long-term stability of encapsulated components.

THIXOTROPIC

ABChimie® 9111 UV LED is thixotropic: it maintains a stable, non-running consistency at rest but flows easily under shear during application. This ensures precise placement, minimal sagging, and uniform coverage before rapid UV curing.

EXCELLENT ADHESION ON FLEXIBLE SUBSTRATES

ABChimie® 9111 UV LED bonds strongly to flexible substrates, including plastics and polymer-based PCBs. Its adhesion ensures reliable protection even on surfaces that bend or flex, ideal for wearables, flexible electronics, and lightweight assemblies.


How to Choose a Resin

Selecting the most suitable resin requires consideration of key factors:

  • ✔ Norms & Compliance
  • ✔ Environment / Exposure Conditions
  • ✔ Repairability
  • ✔ Electrical Performance
  • ✔ Application Method
  • ✔ Operating Temperature

Compliance You Can Trust ✅

ABChimie® 9111 UV LED meets stringent industry standards, ensuring reliability and regulatory adherence for OEMs and contract manufacturers:

  • REACH Compliant
  • RoHS 2011/65/EU Compliant
 

Curing Tip: ABChimie 9111 UV LED cures with UV rays. It is crucial to use the appropriate equipment, as well as the recommended settings, to achieve the best properties of the resin.

Emission Spectrum of Mercury Lamp

PTM6000HV-SP thermal impedance versus bondline thickness

Ref. Leistung / ref power ln % over wavelength in nm

Key Curing Properties

Lamp Type
LED
Emission Spectrum of Mercury Lamp
395 nm
Minimum UVA Dose
-
Coating Thickness
-

Typical property values shown for reference only and should not be used as specifications.




Alternative to LED Lamp Curing of ABChimie 9111 UV LED

ABChimie 9111 UV LED is also available in the mercury version, which cures with a mercury Lamp.

ABChimie 9111 UV [Go to 9111 UV Product Page↗]

  • Thixotropic resin
  • Fluorescent under UV light
  • Excellent adhesion to flexible substrates
  • Immediate curing with UV LED exposure

Best suited for: High-speed process looking to use LED light for curing

Contact Us → 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers