ABLESTIK 958-11
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg
Main features
- Non conductive
- Absorbs stress
- Bonding of large ICs
Product Description
LOCTITE ABLESTIK 958-11 epoxy adhesive is designed to absorb stresses produced when bonding large ICs. It is a non conductive, white die attach that cures with heat and has a pH of ~4 to 9.
Cure Schedule
- 2 hours @ 130°C
- 1 hour @ 150°C
Packaging
Unit of measure Syringe
Net weight 1.8 g
Gross weight 4 g
Dimensions 1.7 x 1 x 6.6 cm
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Work life @25°C
336 hours
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate.
It is based on the change in viscosity and it can rely on the application requirements.
Thermal Properties
Glass Transition Temperature (Tg)
89 °C
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding.
The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
Electrical Properties
Volume Resistivity
500000000000000 Ohms⋅cm
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
Physical Properties
Viscosity
45,000 mPa.s
Viscosity is a measurement of a fluid’s resistance to flow.
Viscosity is commonly measured in centiPoise (cP). One cP is defined as
the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP.
A product like honey would have a much higher viscosity -around 10,000 cPs-
compared to water. As a result, honey would flow much slower out of a tipped glass than
water would.
The viscosity of a material can be decreased with an increase in temperature in
order to better suit an application