LOCTITE ABLESTIK ABP 2032S

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite Ablestik ABP 2032S

Main features

  • Low temperature cure
  • Good adhesion
  • Electrically conductive

Product Description

LOCTITE ABLESTIK ABP 2032S electrically conductive epoxy adhesive is designed as a Pb-free alternative to solder. It cures quickly at low temperatures for good stress control in small to medium die applications. It is a tried and proven product for optical sensor ASIC attach and for Lid attach for optical sensors and 3d sensing modules.

LOCTITE ABLESTIK ABP 2032S has good adhesion and good dispensing characteristics, This material can cure in temperatures as low as 80°C and works great on substrates such as Gold, Steel and Silver. 

Cure Schedule

  • 60 minutes @ 80°C
  • 3 minutes @ 150°C or
  • 10 minutes @ 120°C
Product Family

233348

5cc in 10cc Syringe - 1933176
1. Select Package Type
2. Select Package Size

Loading pricing…

Product availability
US Shipping in 30 days
CA Shipping in 12 weeks
EU Shipping in 35 days
Packaging
Unit of measure Syringe
Net weight 17 g
Gross weight 27 g
Dimensions 9.1 x 2.3 x 3 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
24 hours
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
1 W/m.K
Physical Properties
Thixotropic index
Thixotropic Index is a ratio of a material s viscosity at two different speeds in Ambient temperature, generally different by a factor of ten. A thixotropic material s viscosity will decrease as agitation or pressure is increased. It indicates the capability of a material to hold its shape. Mayonnaise is a great example of this. It holds its shape very well, but when a shear stress is applied, the material easily spreads. It helps in choosing a material in accordance to the application, dispense method and viscosity of a material.
4.5
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
11,000 mPa.s