LOCTITE ABLESTIK ABP 6392TEA

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK ABP 6392TEA

Main features

  • High electrical conductivity
  • High thermal conductivity
  • Good adhesion to a variety of substrates

Product Description

LOCTITE ABLESTIK ABP 6392TEA  electrically and thermally conductive, silver filled die attach paste is specially formulated for high reliability packaging applications. ABLESTIK ABP 6392TEA is designed for use on small to large die sizes to balance stress management.

LOCTITE ABLESTIK ABP 6392TEA adhesive is formulated to provide good adhesion on a wide variety of substrates, including Cu, Ag, PP,F and laminate.

 

Cure Schedule

  • 30 minutes ramp to 175°C + 60 minutes @ 175°C, in air or nitrogen
Product Family

233968

10cc syringe - 2922504
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 23 days
CA Shipping in 2 weeks
EU Shipping in 20 days
Packaging
Unit of measure Syringe
Net weight 39 g
Gross weight 48.74 g
Dimensions 3 x 1.9 x 9.1 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
24 hours
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
56 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
9 W/m.K
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
0.00004 Ohms⋅cm
Chemical Properties
Moisture absorption
0.13 %
Physical Properties
Thixotropic index
Thixotropic Index is a ratio of a material s viscosity at two different speeds in Ambient temperature, generally different by a factor of ten. A thixotropic material s viscosity will decrease as agitation or pressure is increased. It indicates the capability of a material to hold its shape. Mayonnaise is a great example of this. It holds its shape very well, but when a shear stress is applied, the material easily spreads. It helps in choosing a material in accordance to the application, dispense method and viscosity of a material.
5
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
12,500 mPa.s

Additional Information

Recommended Cure Condition

  • 30 minutes ramp to 175°C + 60 minutes @ 175°C, in air or nitrogen.

Thawing

  1. Allow container to reach room temperature before use.
  2. After removing from the freezer, set the syringes to stand vertically while thawing.
  3. Thaw times depend on the syringe size.
  4. Consult handling guide for more information.
  5. DO NOT open the container before contents reach 25°C temperature. Any moisture that collects on the thawed container should be removed prior to opening the container.
  6. DO NOT re-freeze. Once thawed to 25°C, the adhesive should not be re-frozen.

Direction for Use

  1. Thawed material should immediately be placed on dispense equipment for use.
  2. If the adhesive is transferred to a final dispensing reservoir, care must be exercised to avoid entrapment of contaminants and/or air into the adhesive.
  3. Adhesive must be completely used within the product's recommended work life.
  4. Alternate dispense amounts may be used depending on the application requirements.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers