LOCTITE ECCOBOND 50400-1

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Loctite Eccobond 50400-1

Main features

  • Low viscosity
  • Low CTE
  • One component

Product Description

LOCTITE® ECCOBOND 50400-1 glob top is designed for encapsulating wire bonded bare die on epoxy laminate and similar substates. The formulation of this single component material ensures a long pot and a very stable, low viscosity during use.

LOCTITE® ECCOBOND 50400-1 is recommended for use on ICs with high wire profiles and in applications where the spreading of the glob top during cure must be controlled.

 

Cure Schedule

  • 2 hours @ 150°C

Low Stress Cure Schedule

  • 1 hour @ 120°C + 1 hour @ 150°C
Product Family

233325

30cc Syringe - 1425725
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 20 days
Packaging
Unit of measure Syringe
Net weight 40 g
Gross weight 61 g
Dimensions 4 x 3 x 11.8 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
168 hours
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
140 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.63 W/m.K
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
100 mPa.s