HumiSeal Stripper 1063 is a non-acidic liquid stripper for dissolving cured HumiSeal polyurethane conformal coatings from printed wiring board assemblies. The clear product has a specific gravity of 0.84 +/- 0.01, a relative evaporation rate of 2.10, and a TCC flash point of 11.1 deg C. The stated removal process uses a 60 minute immersion, brushing of loosened material, final cleaning with isopropyl alcohol and deionized water or another qualified cleaner, inspection, and a 30 minute bake at 60 to 65 deg C after final cleaning.

Key features

  • Non-acidic polyurethane coating removal: The stripper is formulated to dissolve cured HumiSeal polyurethane conformal coatings.
  • Controlled 60-minute immersion: The documented process uses a one-hour soak before brushing and final cleaning.
  • Clear low-density liquid: The product is supplied as a clear liquid with a specific gravity of 0.84 +/- 0.01.

Applications

  • Removal of cured HumiSeal polyurethane coatings from printed wiring board assemblies
Product Family

HUMISEAL 1063

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Clear
Evaporation Rate
2.1
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.82
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
11.1 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical liquid properties and shelf life before the coating-removal process.

Property Value Unit Method / condition
Appearance Clear liquid - As supplied
Relative evaporation rate 2.10 - Typical liquid value
Specific gravity 0.84 +/- 0.01 - Typical liquid value
Flash point 11.1 deg C TCC
Shelf life 12 months As supplied in the original container