HUMISEAL 2A20

Main features

  • Adhesive and Encapsulant Function
  • 10-Minute Handling Time
  • Mechanical and Thermal Shock Resistance

Product Description

HumiSeal 2A20 is a two-component polyurethane adhesive and encapsulant with matched typical viscosities of 9,000 cP for Part A and Part B. It is a soft, low-viscosity material for general-purpose bonding and encapsulation, with mechanical and thermal shock resistance and adhesion to metals, hard-to-bond plastics, glass, ceramics, polycarbonate, and electronic assemblies. Typical processing times are less than eight minutes of pot life and 10 minutes to handling. Full cure takes 18 hours under room-temperature conditions or 30 minutes at 65 deg C. Applications include electronics, automotive assembly, and industrial work.

Key features

  • Adhesive and Encapsulant Function: The product serves both general-purpose bonding and encapsulation applications.
  • 10-Minute Handling Time: Typical pot life is less than eight minutes.
  • Mechanical and Thermal Shock Resistance: The product has mechanical and thermal shock resistance, with adhesion to multiple substrate types.

Applications

Electronics assembly; automotive assembly; industrial bonding and encapsulation.

Product Family

HUMISEAL 2A20

Loading pricing…

Technical Specifications

General Properties
Component System
Two Part (A/B)

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values from the exact authorized-distributor page for the documented HumiSeal 2A20 configuration.

PropertyValueUnitMethod / condition
ChemistryUrethane-Two-component system; exact distributor page
Part A viscosity9,000cPTypical component value
Part B viscosity9,000cPTypical component value
Pot life<8minutesTypical value
Handling time10minutesTypical value
Technical properties

After-processing / final-state properties

Typical cured-system values from the exact authorized-distributor page; current manufacturer TDS confirmation remains pending.

PropertyValueUnitMethod / condition
Full cure18 hours at RT or 30 minutes at 65 deg C-Exact distributor page
Cure typeTwo-component with heat option-Exact distributor page
ColorClear-Cured system
HardnessShore D45-Cured system
Operating temperature-50 to 100deg CCured system