HumiSeal Thinner 789

Harmonization Code : 3814001000 |

HumiSeal Thinner 789

Main features

  • For use with LTX series of conformal coatings
  • Low odor
  • No aromatic compounds

Product Description

HumiSeal Thinner 789 is developed as a diluent for solvent based conformal coating products. Humiseal Thinner 789 contains no xylene or toluene. It is suitable for use with certain acrylic, polyurethane and synthetic rubber conformal coatings. 

Product Key Features

  • Very low aromatic hydrocarbon content
  • Low odor 

Applications

  • Specifically designed for the use with the LTX series conformal coatings.
Product Family

234437

1-Liter Can
1. Select Package Size

Loading pricing…

Product availability
EU Shipping in 6 weeks
Packaging
Unit of measure Bottle
Net weight 1 kg
Gross weight 1.1 kg
Dimensions 7.3 x 6 x 11.6 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Clear
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.75
Vapor Pressure
0.0132563 kg/cm2
Thermal Properties
Boiling Point
The amount of degree’s needed to reach in order to make the substance boil.
140 °C
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
26 °C

Additional Information

Cautionary Statement

Application of HumiSeal® Conformal Coatings should be carried out in accordance with local and National Health and Safety regulations.  

The solvents in HumiSeal® Conformal Coatings are flammable. Material should not be used in presence of open flame or sparks. Use only in well-ventilated areas to avoid inhalation of vapours or spray.  Avoid contact with skin and eyes. Consult SDS prior to use.  