CC-SAC305 | Copper Core SAC 305 Solder spheres

Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

CC-SAC305 | Copper Core SAC 305 Solder spheres

Main features

  • SAC 305 alloy
  • Core of the sphere is Copper
  • Excellent fatigue resistance

Product Description

LINQALLOY CC-SAC305 solder Spheres are lead-free Tin/Silver/Copper alloys that contain 96.5% Tin (Sn), 3% Silver (Ag), and 0.5% Copper (Cu) and is often written as Sn96.5Ag3.0Cu0.5. These are not the normal SAC305 spheres since they have a copper core that enables "no tilt" designs and can act as a spacer for applications that require perfect BLT control. The size of the core depends on the diameter of the sphere.

LINQALLOY CC-SAC305 offers has excellent fatigue resistance and it is compatible with all flux types. It exhibits excellent joint reliability and it is the best wetting Sn/Ag/Cu alloy in the market.

Each jar has a clear label on the lid specifying the solder ball diameter as well as a label on the front identifying the alloy type, the quantity of spheres in the jar, the date of manufacture, and the product lot (or batch) number. This batch number is also tied to a certificate of conformance that is also provided with the solder spheres and ensures the SAC305 solder spheres meet the following quality criteria:

  • Tin (Sn): 96.5%
  • Silver (Ag): 3%
  • Copper (Cu): 0.5%
  • Melting Temperature (Solidus): 217°C
  • Melting Temperature (Liquidus): 219°C
  • Sphericity: Within 1.5%

Diameter Tolerance

  • 0.22mm - 0.48mm (220µm - 480µm) : ± 0.010mm (± 10µm)
  • 0.50mm - 0.762mm (500µm - 762µm) : ± 0.025mm (± 25µm)

Sphere diameter and Copper Core size reference

  • 60 µm – 100 µm Core Copper
  • 110 µm – 150 µm Core Copper
  • 210 µm – 250 µm Core Copper
Product Family

233674

0.150mm (5.9mil) | 1,000,000 spheres
1. Select Diameter
2. Select Package Size

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Jar
Net weight 0.0131 kg
Gross weight 0.0144 kg
Dimensions 6 x 6 x 10 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Alloy Type
A metallic element type
SAC305
Density (g)
7.4 g/cm3
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
37 %
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
71.8 W/m.K

Additional Information

What do I get when I buy CC-SAC305 Eutectic Solder Spheres from KRAYDEN?

The advantage of ordering solder spheres online at KRAYDEN.com is that you can be sure of the quality. The solder spheres you receive are originally manufactured solder spheres packed into jars with inert gas (nitrogen). We do not repack the solder balls we receive, so the jars you will receive have never been opened, thus ensuring the quality of the product you receive. The lid of the jar is also always sealed with a shrink-wrapped plastic wrap ensuring that the solder spheres do not oxidate in the jar.

 

Presentation

 

 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers