SAC125N | PbFree Solder Spheres

Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

SAC125N Lead-Free Solder Spheres

Main features

  • Lead-Free Solder Spheres
  • Lowest cost Sn/Ag/Cu Alloy
  • Nickel Dopped, hence the SACNi name

Product Description

LINQALLOY SAC125N Solder Spheres are lead-free Tin/Silver/Copper alloys that contain 98.3% Tin (Sn), 1.2% Silver (Ag), 0.5% Copper (Cu) and 0.05% Nickel (Ni) and is often written as Sn98.3Ag1.2Cu0.5 and called SAC125Ni. SAC125N Solder Spheres contain a small amount of Nickel for anti-oxidation and are used by companies working with BGA, CSP, LBGA, PBGA and CBGA components who have made the transition to Lead-free (Pb-free) soldering.

Features:

  • Lowest Cost Sn/Ag/Cu Alloy
  • Excellent Fatigue Resistance
  • Compatible with all Flux Types
  • Excellent Solder Joint Reliability
  • Best Wetting Sn/Ag/Cu Alloy
  • Nickel Doped, hence the SAC125Ni name

 

Furthermore, each jar has a clear label on the lid specifying the solder ball diameter as well as a label on the front identifying the alloy type, the quantity of spheres in the jar, the date of manufacture, and the product lot (or batch) number. This batch number is also tied to a certificate of conformance that is also provided with the solder spheres and ensures the SAC105 solder spheres meet the following quality criteria:

  • Tin (Sn): 98.3%
  • Silver (Ag): 1.2%
  • Copper (Cu): 0.5%
  • Nickel (Ni): 0.05%
  • Melting Temperature (Solidus): 217°C
  • Melting Temperature (Liquidus): 219°C
  • Sphericity : Within 1.5%

Diameter Tolerance

  • 0.22mm - 0.48mm (220µm - 480µm) : ± 0.010mm (± 10µm)
  • 0.50mm - 0.762mm (500µm - 762µm) : ± 0.025mm (± 25µm)
Product Family

233140

Alloy: Sn98.3/Ag1.2/Cu0.5/Ni0.005 » 0.300mm (12mil) » 250,000 spheres
1. Select Diameter
2. Select Package Size

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Jar
Net weight 0.0259 kg
Gross weight 0.0285 kg
Dimensions 6 x 6 x 10 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Alloy Composition
Composition of the alloy material
SAC125Ni
Alloy Type
A metallic element type
SAC125N
Spheroid Tolerance
The allowed % that a solder ball (solder sphere) can divert from being perfectly round and spherical. We take one lot of solder spheres and divide it into 4 smaller lots. Each lot is then checked with advanced visual inspection systems. If even 1 ball is out of spec, the entire batch is scrapped and reworked!
1.5 %
Other Properties
RoHS Compliant
RoHS is a product level compliance based on a European Union Directive which restricts the Use of certain Hazardous Substances in Electrical and Electronic Equipment (RoHS). Products compliant with this directive do not exceed the allowable amounts of the following restricted materials: lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls (PBB) and polybrominated diphenyl ethers (PBDE), with some limited exemptions
Yes

Additional Information

What do I get when I buy SAC125N Solder Spheres from KRAYDEN?

The advantage of ordering solder spheres online at KRAYDEN.com is that you can be sure of the quality. The solder spheres you receive are originally manufactured solder spheres packed into jars with inert gas (nitrogen). We do not repack the solder balls we receive, so the jars you will receive have never been opened, thus ensuring the quality of the product you receive. The lid of the jar is also always sealed with a shrink-wrapped plastic wrap ensuring that the solder spheres do not oxidate in the jar.

Presentation

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers