LINQCELL CF350 | 350um Carbon Fabric

Harmonization Code : 6815.11.00.00 | Articles of stone or of other mineral substances, not elsewhere specified or included; Non-electrical articles of graphite or other carbon; Carbon fibres and articles of carbon fibres

LINQCELL CF350 | 350um Carbon Fabric

Main features

  • 0.35mm - 350um - 14mil
  • Comes in roll form
  • 5 TP Resistance

Product Description

LINQCELL CF350 is a 0.35mm thick carbon cloth without a Microporous layer and PTFE. It is commonly used as a gas diffusion layer and electrode for fuel cells. Its through-plane resistivity is less rhN 5 mΩcm2.

LINQCELL CF350 carbon cloth is typically used in PEM fuel cells as well as Phosphoric acid fuel cells and Direct methanol fuel cell applications as a gas diffusion layer. Carbon cloth based GDLs have performance equal to that of conventional carbon papers. Carbon cloth is more practical than carbon paper because of its superior compressibility, elasticity, and flexibility performance, making it more appropriate for ongoing manufacturing and assembly processes. 

These thinner gas diffusion layers lend themselves better to AEMFC GDL Anodes. Thickness has more sensitivity to the AEMFC when used in the anode electrode rather than in the cathode electrode, indicating that water removal at the anode was more challenging than water supply at the cathode so the strategy of water management among electrodes should be differentiated.

Product Family

233778

50cm x 200cm | Roll form
1. Select Sheet Size

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Roll
Net weight 0.56 kg
Gross weight 0.616 kg
Dimensions 200 x 50 x 0.035 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Basis Weight
Basis weight refers to the weight measured in pounds off 500 sheets of paper in that paper’s basic sheet size.
130 g/m2
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
360 μm
Electrical Properties
TP Resistance
Opposition to the flow of electric current.
5 mΩcm2
Mechanical Properties
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
10 N/cm

Additional Information

Please note that the thickness can easily vary ±10-20um