LINQCELL GDL1500 | 1.5mm Carbon Plate

Harmonization Code : 6815.11.00.00 | Articles of stone or of other mineral substances, not elsewhere specified or included; Non-electrical articles of graphite or other carbon; Carbon fibres and articles of carbon fibres

GDL1500 | 1.5mm Carbon Plate

Main features

  • 1.5mm - 1500um - 59mil
  • Alternative to Spectracarb 6060
  • Graphitized Carbon Plate

Product Description

LINQCELL GDL1500 is a graphitized carbon plate, commonly used as a gas diffusion layer and electrode for fuel cells. Its through plane resistance is less than 13.5 mΩcm2. The thickness is 1.5mm and is measured at 50 kpa. This material has been successfully used in assemblies for hydrogen production electrolyzer components as a gas diffusion layer and electrode.

LINQCELL GDL1500 with a density of ±0.60 g/cm3 is a close, almost direct, alternative to the highly popular and discontinued Spectracarb 6060. Compared to it it has a resistivity of 90mΩ-cm instead of 100mΩ-cm. Shortly, we should be able to die cut circles and most designs that you might require.

Air permeability of LINQCELL GDL1500 was evaluated using the ISO 5636-5 standard test method. Using a sample area of 0.1 in2 and an air volume of 300 mL, the measured air passage times were 9.30 s, 9.45 s, and 8.88 s (average: ~9.2 s).

Product Family

231001

400 x 400mm Sheet
1. Select Sheet Size

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Sheet
Net weight 0.02 kg
Gross weight 0.022 kg
Dimensions 40 x 40 x 1.5 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Basis Weight
Basis weight refers to the weight measured in pounds off 500 sheets of paper in that paper’s basic sheet size.
858 g/m2
Density (g)
0.60 g/cm3
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
1500 μm
Electrical Properties
Through Plane Resistivity
Resistance of the amount of current through a material
90.6 mΩcm
TP Resistance
Opposition to the flow of electric current.
13.3 mΩcm2
Voltage loss
24.5 mV

Leading Brands Trust in Our Products and Services