LINQCELL GDL1500B | 1.5mm Carbon Plate

Harmonization Code : 6815.11.00.00 | Articles of stone or of other mineral substances, not elsewhere specified or included; Non-electrical articles of graphite or other carbon; Carbon fibres and articles of carbon fibres

LINQCELL GDL1500B | 1.5mm Carbon Plate LINQCELL GDL1500B | 1.5mm Carbon Plate

Main features

  • 1.5mm - 1500um - 59mil
  • Alternative to Spectracarb 6060
  • Improved compressibility

Product Description

LINQCELL GDL1500B is a graphitized carbon plate that boasts impressive technical specifications, making it an excellent choice for use in PEM electrolyzers, PEMFCs, and PAFCs. This carbon paper is commonly used as a gas diffusion layer, porous transport layer and electrode, making it a versatile option for various fuel cell applications.

One of the most notable features of LINQCELL GDL1500B is its low electrical resistance, with a through-plane resistance of less than 21 mΩcm2. This means that it can conduct electricity with high efficiency, making it a reliable and cost-effective choice for fuel cells. Additionally, it has high thermal conductivity, allowing it to transfer heat effectively under high-temperature conditions.

Another key feature of this carbon paper is its high compressibility, which enables it to reach ~1.3mm at 2MPa. This ensures excellent contact with the catalyst layer, promoting optimal performance. Moreover, its durability and low corrosion rate make it a reliable option that can last for extended periods.

LINQCELL GDL1500B is a close alternative to the highly popular and discontinued Spectracarb 6060. This B version retains good strength while having significantly improved compressibility over the original GDL1500 product. It can reach ~1.3mm at 2MPa. It is not only a suitable choice for an electrode or gas diffusion layer, but it also works excellently as a Porous Transport Layer (PTL) in fuel cells. Its high compressibility and porosity allow for optimal reactant transport to the catalyst layer, which is crucial for high-performance fuel cells and electrolyzers.

Applications: PEM Electrolyzers, PEMFCs and PAFCs in distributed power generators

Key Features:

  • High compressibility (>0.3mm at1.5Mpa) 
  • High thermal conductivity 
  • Low electrical resistance
  • Applicable under high temperature
  • High durability and low corrosion

Typically thicker carbon plates such as GDL1500B are specifically suitable for Electrolyzers.

Product Family

233752

400 x 400mm Sheet
1. Select Sheet Size

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Sheet
Net weight 1.884 kg
Gross weight 2.0724 kg
Dimensions 40 x 40 x 0.15 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Basis Weight
Basis weight refers to the weight measured in pounds off 500 sheets of paper in that paper’s basic sheet size.
670 g/m2
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
1500 μm
Electrical Properties
Through Plane Resistivity
Resistance of the amount of current through a material
140 mΩcm
TP Resistance
Opposition to the flow of electric current.
21 mΩcm2
Voltage loss
39 mV

Additional Information

 General Function-Related Properties For GDL

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers