LINQCELL GDL2900 | 2.9mm Carbon Plate

Harmonization Code : 6815.11.00.00 | Articles of stone or of other mineral substances, not elsewhere specified or included; Non-electrical articles of graphite or other carbon; Carbon fibres and articles of carbon fibres

GDL2900 | 2.9mm Carbon Plate

Main features

  • 2.9mm - 2900um - 114mil
  • Thickest GDL available
  • Graphitized Carbon Plate

Product Description

LINQCELL GDL2900 is a graphitized carbon plate, commonly used as a gas diffusion layer and electrode for fuel cells. Its through plane resistance is less than 25 mΩcm2.  It has a thickess of 2.9mm that is measured at 50 kpa.

LINQCELL GDL2900 has a density of ±0.60 g/cm3 and a through plane resistivity of 90mΩ-cm instead of 100mΩ-cm from the classic Spectracarb grades. Voltage loss is 28mV. Shortly, we should be able to die cut circles and most designs that you might require. 

Product Family

231003

400 x 400mm Sheet
1. Select Sheet Size

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Sheet
Net weight 0.02 kg
Gross weight 0.022 kg
Dimensions 40 x 40 x 0.5 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Basis Weight
Basis weight refers to the weight measured in pounds off 500 sheets of paper in that paper’s basic sheet size.
1734 g/m2
Density (g)
0.60 g/cm3
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
2900 μm
Electrical Properties
Through Plane Resistivity
Resistance of the amount of current through a material
87.5 mΩcm
TP Resistance
Opposition to the flow of electric current.
24.5 mΩcm2
Voltage loss
27 mV