LINQCELL GDP210-MPS | 210um Carbon Paper

Harmonization Code : 6815.11.00.00 | Articles of stone or of other mineral substances, not elsewhere specified or included; Non-electrical articles of graphite or other carbon; Carbon fibres and articles of carbon fibres

LINQCELL GDP210-MPS | 210um Carbon Paper

Main features

  • 0.21mm - 210um - 8.2mil
  • Treated at 2000 °C
  • With MPL and Hydrophobic coating

Product Description

LINQCELL GDP210-MPS is a 210-µm thick graphitized carbon fiber paper made from high-quality polyacrylonitrile (PAN) fibers. The fibers undergo a wet-laying process to form a non-woven, fibrous, and porous structure, which is then carbonized and graphitized. The material undergoes high-temperature graphitization at 2000 °C, resulting in superior electrical conductivity, high oxidation resistance, and excellent thermal stability. This elevated temperature further enhances the electrical performance and compressibility of the material compared to the standard LINQCELL GDP210-MP (produced at 1600 °C), although it significantly increases production costs. LINQCELL GDP210-MPS is particularly recommended when minimizing resistivity is critical. It is an excellent choice as a gas diffusion layer in fuel cells and as a gas diffusion substrate for carbon dioxide electrolyzers. You can check our blog to find out how graphitization affects the structure and properties of carbon papers. 

LINQCELL GDP210-MPS has a microporous layer and PTFE coating, which provide hydrophobicity and increased surface area. The higher surface area maximizes catalyst utilization, which increases fuel cell efficiency. Meanwhile, the hydrophobic properties improve water removal and ensure stable operation by preventing flooding within the stack. 

Key Features:

  • 210-µm Thickness: Optimized for reduced stack volume and internal resistance.
  • High-Temperature Graphitization (2000 °C): Provides excellent electrical conductivity, oxidation resistance, and thermal stability.
  • Microporous Layer & PTFE Coating: Enhances hydrophobicity, increases surface area, and optimizes catalyst utilization.
  • Improved Water Management: Hydrophobic properties prevent flooding and ensure stable operation by enhancing water removal.
  • High Compressibility and Porosity: Can be compressed down to 120 µm at 3.5 MPa (350 N/cm2).

Highly Recommended As:

LINQCELL GDP210-MPS is available in sheet form only. LINQCELL Graphitized Carbon Fiber Papers with MPL and PTFE treatment are offered in a standard width of 40 cm. Contact us for custom sizes or other specific requirements.

Product Family

233774

40 X 40 Sheet
1. Select Sheet Size

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Sheet
Net weight 0.144 kg
Gross weight 0.1584 kg
Dimensions 40 x 40 x 0.3 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Basis Weight
Basis weight refers to the weight measured in pounds off 500 sheets of paper in that paper’s basic sheet size.
90 g/m2
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
210 μm
Electrical Properties
TP Resistance
Opposition to the flow of electric current.
6.5 mΩcm2
Voltage loss
14 mV
Other Properties
Air Permeability
225 seconds
Mechanical Properties
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
27 N/cm

Additional Information

LINQCELL GDP210-MPS Compressibility

GDP210-MPS Thickness vs Compression Pressure
GDP210-MPS Compressibility vs Compression Pressure

 

GDP210-MPS Electrochemical Performance

Test Settings
Reaction Area [cm2] 300
Fuel Supply Method Constant Flow
Relative Humidity [%] 100
Test Temperature [°C] 60
Anode Chemical Dose Ratio 1.5 splm (H2, 100% RH)
Cathode Chemical Dose Ratio 2.5 splm (Air, 100% RH)
Operating Pressure 10 psi
Clamping Pressure 10 psi
 GDP210MPS Electrochemical Performance

 