LINQCELL VRB-AEM50

Harmonization Code : 3920.99.53 | Other plates, sheets, film, foil and strip, of plastics, non-cellular and not reinforced, laminated, supported or similarly combined with other materials ; Of other plastics ; Ion-exchange membranes of fluorinated plastic material, for use in chlor-alkali electrolytic cells

LINQCELL VRB-AEM50

Main features

  • 50um - Low ohmic resistance
  • Excellent oxidative stability and chlorine resistance
  • Designed as ion exchange membranes for redox flow batteries

Product Description

LINQCELL VRB-AEM50 is a 50-µm partially fluorinated anion exchange membrane without reinforcement. It has low ohmic resistance, excellent mechanical properties, low water uptake, and minimal dimensional swelling. VRB-AEM50 has high oxidative stability, resists chlorine, and remains stable in acidic environments (pH > 4). The recommended operating temperature is from room temperature to 50 °C.

LINQCELL VRB-AEM50 is highly suitable for electrochemical applications that require exceptional oxidative stability and chlorine resistance, such as redox flow batteries operating with very harsh, aqueous acidic solutions.

Key Features and Benefits:

  • Low Resistance: Facilitates efficient ion transport, minimizing energy losses and maximizing device performance.
  • High Vanadium Ion Blocking Capability: Significantly reduces vanadium crossover in Redox-Flow Batteries, ensuring prolonged operational lifespan and enhanced efficiency.   
  • High Acidic Stability: Maintains its integrity and performance in harsh acidic conditions, crucial for applications like Vanadium-Redox-Flow Batteries (VRBs).

Highly Recommended for:

  • Vanadium-Redox-Flow Batteries (VRBs)
  • Aqueous Acidic Redox-Flow Batteries.

LINQCELL VRB-AEM50 comes in different sizes to meet various device design requirements. Contact us for custom sizes or other specific requirements.

Product Family

234006

40x250 cm Sheet | 1m²
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Roll
Net weight 0.01 kg
Gross weight 0.012 kg
Dimensions 40 x 250 x 1 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Transparent
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
44 - 56 μm
Physical Properties
Young's modulus
750 MPa

Additional Information

LINQCELL VRB-AEM50 Properties

Property Value Unit
Initial Form Dry film with no counter-ions —
Backing Foil Polyethylene terephthalate (PET) —
Area-specific Resistance in 0.5M H2SO4 < 0.5 Ω•cm2
Ion Selectivity 0.1/0.5 mol/kg KCl at 25°C > 90 %
Swelling Ratio in 2M H2SO4 at 25°C < 16 %

 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers