LOCTITE EDAG 7019 E&C

Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category

LOCTITE EDAG 7019 E&C

Main features

  • Flexible
  • Good adhesion
  • Medical grade

Product Description

LOCTITE EDAG 7019 E&C is a blend of finely divided silver and silver chloride particles in a thermoplastic resinIt is formulated to provide excellent adhesion to the wide variety of substrates used in the manufacture of electrically conductive medical devices.

LOCTITE EDAG 7019 E&C is a flexible conductive ink with low electrical resistance and long screen residence time. It can be cured with hot air drying and heat cure.

 

Cure Schedule

  • 10 minutes @ 107°C or

 

 

Product Family

233636

0.5Kg Jar - 1263544
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 23 days
CA Shipping in 12 weeks
EU Shipping in 40 days
Packaging
Unit of measure Jar
Net weight 1 kg
Gross weight 1.154 kg
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
63.3 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
14,000 mPa.s