Lubricating Oils & Dispersions

Synthetic, mineral & colloidal systems

Lubricating Oils & Dispersions

Lubricating oils and liquid dispersions represent the primary line of defense against mechanical friction, surface wear, and thermal degradation in moving mechanical assemblies. A lubricating oil is a fluid tribological medium engineered to physically separate contacting surfaces in motion, minimize energy dissipation caused by friction, transport heat away from high-stress friction zones, and carry away wear debris. Liquid dispersions advance this functionality by suspending sub-micron or micron-sized solid lubricant particles—such as Molybdenum Disulfide (MoS2), Polytetrafluoroethylene (PTFE), Synthetic Graphite, or Hexagonal Boron Nitride (h-BN)—within a liquid carrier phase. This ensures continuous boundary-film protection under extreme-pressure (EP) conditions, where conventional liquid films collapse.

From high-speed precision machine tool spindles and heavy industrial gearboxes to complex hydraulic systems and automotive powertrains, selecting the correct liquid lubricant chemistry directly dictates equipment reliability, operational efficiency, and mean time between failures (MTBF). Modern industrial applications demand tailored fluid formulations capable of operating across broad thermal spans (-60°C to >300°C), ultra-high mechanical shear rates, and aggressively corrosive chemical environments.

35 products

  • Dow XIAMETER PMX 200

    XIAMETER PMX 200

    • 1,000 cSt Polydimethylsiloxane Fluid
    • Surface Tension of 21.2 dynes/cm
    • Dielectric Strength of 400 volts/mil
  • BONDERITE L-FG LS2127

    BONDERITE L-FG LS 2127

    • Up to 1649 deg C Service
    • Anti-Stick Non-Ferrous Tooling Coating
    • Brush, Spray, or Dip Application
  • DOWSIL 710

    DOWSIL 710

    • Up to 260 deg C Closed-System Service
    • Low-Volatility Oxidation-Resistant Fluid
    • High-Temperature Lubrication/Heat-Transfer Applications
  • LOCTITE LB8023

    LOCTITE LB8023

    • Calcium-Sulfonate Grease Formulation
    • High-Lubricity Thread Assembly
    • Galvanic Corrosion Prevention
  • MOLYKOTE 7400

    MOLYKOTE 7400

    • Water-Based MoS2/Graphite Dry-Film Lubricant
    • High Load-Carrying Capacity
    • Air-Curing Lubricant Coating
  • MOLYKOTE CU-7439

    MOLYKOTE CU-7439

    • Up to 650 deg C Service
    • High-Adhesion Copper Paste
    • Nondestructive Thread-Disassembly Support
  • MOLYKOTE L-1268

    MOLYKOTE L-1268

    • Fully Synthetic ISO Vg 68 PAO Lubrication
    • 54 deg C Pour Point
    • Longer Oil-Drain Intervals
  • MOLYKOTE L-1468 FM

    MOLYKOTE L-1468 FM

    • ISO VG 68 PAO Chain Oil
    • Freezer-Chain Anti-Wear Lubrication
    • NSF H1 Registration
  • MOLYKOTE L-1668FM

    MOLYKOTE L-1668FM

    • ISO Vg 68 Mineral-Oil
    • Low Vapor Pressure
    • Carries NSF H1 Certification
  • BONDERITE L-GP-D148A

    BONDERITE L-GP-D148A

    • PTFE Dry-Film Lubricant Formation
    • Spray-Viscosity Thinning Compatibility
    • Room-Temperature Cure with Heat Acceleration
  • LOCTITE 8060

    LOCTITE 8060

    • High-Temperature Anti-Seize Protection
    • Controlled Stick Application
    • Measured Assembly Torque Behavior
  • LOCTITE LB8017

    LOCTITE LB8017

    • Multi-Method Dry-Film Application
    • 400 deg C Sliding Service
    • 1315 deg C Anti-Seize Range
  • LOCTITE LB8504

    LOCTITE LB8504

    • Non-Metallic Conductive Anti-Seize
    • 482 deg C Operating Range
    • 0.13 Steel Fastener Torque Coefficient
  • LOCTITE LB8213

    LOCTITE LB 8213

    • 0.362 mm Four-Ball Wear Scar
    • -26 to 260 deg C Operating Range
    • PFPE/PTFE NLGI 2 Grease
  • MOLYKOTE L-0268

    MOLYKOTE L-0268

    • Corrosion-Inhibited Process-Gas Lubrication
    • ISO 68 Compressor-Oil Selection
    • Controlled Oxygen-Service Boundary
  • MOLYKOTE L-0322

    MOLYKOTE L-0322

    • ISO 22 Hydraulic-Fluid Selection
    • Rust-Oxidation and Anti-Wear Additives
    • Low-Viscosity Hydraulic System Service
  • MOLYKOTE L-0346

    MOLYKOTE L-0346

    • ISO 46 Hydraulic-Fluid Selection
    • Rust-Oxidation and Anti-Wear Additives
    • Medium-Viscosity Hydraulic System Service
  • MOLYKOTE L-1115FM

    MOLYKOTE L-1115FM

    • ISO VG 150 gear oil
    • Synthetic PAO performance
    • Food-grade
  • MOLYKOTE L-1122FM

    MOLYKOTE L-1122FM

    • NSF H1 Food-Machinery Lubrication
    • ISO 220 PAO Gear Lubrication
    • High-Load Oxidation Resistance
  • MOLYKOTE L-1132FM

    MOLYKOTE L-1132FM

    • ISO VG 320 Gear-Oil Viscosity
    • PAO Gearbox Lubrication
    • Food-Processing Gear Service
  • MOLYKOTE L-1146FM

    MOLYKOTE L-1146FM

    • High-Viscosity Gearbox Lubrication
    • PAO Viscosity Index 152
    • Food-Processing Gear Service
  • MOLYKOTE L-1210

    MOLYKOTE L-1210

    • ISO VG 100 Compressor Lubrication
    • PAO Wide-Temperature Viscosity
    • Rust and Oxidation Protection
  • MOLYKOTE L-1232

    MOLYKOTE L-1232

    • ISO VG 32 Compressor Oil
    • PAO Low-Temperature Flow
    • Rust and Oxidation Protection
  • MOLYKOTE L-1232FM

    MOLYKOTE L-1232FM

    • ISO VG 32 Compressor Lubrication
    • PAO Low-Temperature Flow
    • Food-Grade Compressor Oil Identity
  • MOLYKOTE L1246

    MOLYKOTE L-1246

    • ISO VG 46 Compressor Lubrication
    • PAO Low-Temperature Flow
    • Rust and Oxidation Protection
  • MOLYKOTE L1246FM

    MOLYKOTE L-1246FM

    • NSF H1 Compressor Lubrication
    • Temperature-Indexed PAO Viscosity
    • Food-Machinery Lubrication Scope
  • MOLYKOTE L-1428

    MOLYKOTE L-1428

    • High-Temperature Chain Lubrication
    • High-Viscosity Chain-Oil Profile
    • Rust and Anti-Wear Additives
  • MOLYKOTE L-1510

    MOLYKOTE L-1510

    • Corrosive-Gas Compressor Lubrication
    • Wide-Range ISO VG 100 Stability
    • Clear Oxygen-Service Boundary
  • MOLYKOTE L-1568

    MOLYKOTE L-1568

    • Lower-Viscosity Process-Gas Lubrication
    • Wide-Range PAO Viscosity Control
    • Defined Oxygen-Service Limit
  • MOLYKOTE L-2115

    MOLYKOTE L-2115

    • Extreme-Pressure Enclosed-Gear Lubrication
    • Micropitting-Focused PAO Protection
    • Rapid 10-Minute Water Separation
  • MOLYKOTE L-2122

    MOLYKOTE L-2122

    • Stable ISO VG 220 Gear Lubrication
    • Micropitting Protection in Severe Conditions
    • High FZG Load-Carrying Performance
  • MOLYKOTE L-2132

    MOLYKOTE L-2132

    • High-Viscosity Enclosed-Gear Lubrication
    • Corrosion-Inhibited EP Formulation
    • Severe-Condition Micropitting Protection
  • MOLYKOTE L-3246

    MOLYKOTE L-3246

    • Wide-Temperature PAG/POE Viscosity
    • Oxidation-Resistant Compressor Lubrication
    • Rotary-Screw Compressor Fit
  • MOLYKOTE L-4611

    MOLYKOTE L-4611

    • Dedicated Reciprocating-Compressor Lubrication
    • Temperature-Indexed Diester Viscosity
    • Rust and Oxidation Protection
  • MOLYKOTE L-8030

    MOLYKOTE L-8030

    • Non-Sticky Semi-Dry Lubrication
    • Tested Plastic-Contact Compatibility
    • Low-Friction Sliding Performance

Frequently asked questions

Q1: What is the fundamental difference between a pure lubricating oil and a solid-in-oil dispersion?

A pure lubricating oil relies entirely on its hydrodynamic and elastohydrodynamic liquid film thickness, supplemented by dissolved chemical anti-wear (AW) or extreme-pressure (EP) additives (e.g., ZDDP, sulfur-phosphorus compounds). A colloidal dispersion contains insoluble solid lubricant micro-particles suspended homogeneously in the carrier oil. When heavy shock loads collapse the liquid oil film, these solid particles physically deposit on surface asperities to prevent catastrophic metal-to-metal welding and scuffing.

Q2: How do solid particles in colloidal dispersions remain in suspension without settling down over time?

Suspension stability is achieved through sub-micron particle size reduction (typically 0.1 to 2.0 microns), Brownian motion, and steric or electrostatic stabilization techniques. Polymeric dispersants and surfactant additives are coated onto the particle surfaces to generate repelling forces that exceed gravitational sedimentation forces, matching Stokes' Law parameters for colloidal permanence.

Q3: Are synthetic oils always superior to mineral oils?

Synthetic base oils (PAO, PAG, Synthetic Esters, Silicone) provide higher Viscosity Index (VI), exceptional thermal stability, lower pour points, and lower volatility compared to Group I-III mineral oils. However, mineral oils offer excellent seal compatibility, high natural solvency for additives, and cost-efficiency for lower-temperature, non-extreme applications.

Q4: Can I mix Polyalkylene Glycol (PAG) oil with Polyalphaolefin (PAO) or Mineral oils?

No. Conventional PAG base fluids are immiscible with Mineral oils and PAOs. Mixing them leads to phase separation, additive precipitation, severe sludge formation, and filter clogging. Water-insoluble PAGs exist, but cross-contamination should strictly be avoided without explicit engineering validation.

Q5. Is a higher-viscosity oil always more protective?

No. Higher viscosity can increase film thickness, but it also increases churning, pumping and viscous drag, reduces low-temperature flow and may starve a contact if the oil cannot reach the inlet quickly enough. Too-low viscosity can produce insufficient film and high leakage. The correct target is the viscosity range required at operating temperature and speed, with enough margin for load, temperature excursions and ageing.

Q6. What does ISO VG mean?

ISO VG is a viscosity classification for industrial liquid lubricants. The grade number corresponds to the nominal kinematic viscosity at 40 degrees C; it does not identify base oil, additive system, quality level or application approval. ISO 3448 creates a common viscosity language, but two fluids with the same ISO VG can perform very differently.

Q7. Will solid particles in a dispersion damage a bearing or block a filter?

They can if particle size, hardness, agglomeration or concentration is wrong for the contact and delivery system. A useful particle additive must remain dispersed, be small enough for clearances and filters, and produce a beneficial surface or transfer-film effect under the actual tribological conditions. Do not bypass filtration or raise particle limits solely to accommodate a dispersion without a validated engineering review.

 

Learn more

Anatomic Composition of Oil Formulations

Lubricating oils and liquid dispersions consist of three core components formulated to achieve target tribological properties.

Base Oil Matrix

75% – 99%

The base fluid supplies most of the volume and establishes liquid film thickness, cooling efficiency, flow dynamics, and basic hydrodynamic load capacity. Common families include refined mineral oil, hydrocracked mineral base stocks, PAO, esters, PAG, alkylated aromatics, silicones, PFPE, and vegetable-derived esters.

Chemical Additive Package

1% – 20%

Additives work at far lower concentration than the base fluid but control decisive failure modes: antioxidants slow chemical aging, corrosion inhibitors protect wet surfaces, anti-wear and EP additives form sacrificial films, and detergents, demulsifiers, viscosity modifiers, and pour-point depressants manage deposits, water separation, and low-temperature flow.

Dispersed Solid Phase

0.5% – 10% in dispersions

Adds a third design layer, the particle-plus-interface. Lamellar solids such as MoS2 and graphite shear along preferred planes; PTFE contributes low shear and transfer-film behavior; surfactants and dispersants supply electrostatic or steric stabilization.

Solid-lubricant dispersions differ from a pure liquid oil by suspending sub-micron solid particles directly in the fluid matrix. Where a pure oil relies entirely on dissolved chemistry and film thickness, a dispersion adds a physical, mechanical barrier that continues to protect surfaces even after the liquid film has locally collapsed.

Stability should be assessed over realistic time and temperature, not only from the appearance of a freshly sonicated sample, using checks such as sediment height, re-dispersibility, particle-size distribution, and centrifuge screening.

Pure lubricating oil vs colloidal liquid dispersion composition

API Base Oil Classification Rules

API base oil groups overview

Because the base oil constitutes 70% to 99% of a finished lubricant, its chemical purity and molecular structure dictate the baseline performance of the fluid, specifically its thermal stability, oxidation resistance, and low-temperature fluidity.

The American Petroleum Institute (API) categorizes base stock oils into five groups based on refining methods, saturation levels, sulfur content, and viscosity index (VI).

API Group Saturates (%) Sulfur (%) Viscosity Index (VI) Manufacturing & Structure
Group I < 90 > 0.03 80 to 119 Solvent refining; aromatic heavy hydrocarbon mixture.
Group II ≥ 90 ≤ 0.03 80 to 119 Hydrocracking & hydrotreating; lower aromatics.
Group III ≥ 90 ≤ 0.03 ≥ 120 Severe isomerization hydrocracking; paraffinic synthesis.
Group IV 100 0 130 to 180 Polyalphaolefins (PAO); synthesized oligomerization of 1-decene.
Group V Variable Variable Up to >220 All synthetics outside Group IV (esters, PAG, silicone, PFPE, AN).

Group I: Legacy Mineral Oils

Chemistry: Manufactured using older solvent-refining processes, with a high percentage of unstable aromatic compounds and sulfur.

Applications: General-purpose circulating oils, older marine engines, heavily formulated metalworking fluids.

Group II: Modern Industrial Workhorse

Chemistry: Manufactured via hydrotreating and hydrocracking, breaking down aromatics and removing sulfur.

Applications: Modern hydraulic fluids (ISO VG 32–68), industrial gear oils, standard automotive engine oils.

Group III: Highly Refined "Synthetics"

Chemistry: Severe hydrocracking and catalytic dewaxing restructure hydrocarbons into stable paraffinic chains.

Applications: High-performance compressor oils, premium turbine oils, top-tier automotive lubricants.

Group IV: Polyalphaolefins (PAO)

Chemistry: Fully synthetic; built by oligomerizing ethylene gas into 1-decene, then synthesized into PAO.

Applications: Extreme-cold hydraulics, high-speed CNC spindles, heavy-duty synthetic gear oils.

Group V: Specialty Synthetics

Chemistry: A catch-all category for base stocks that don't fit into Groups I through IV, including esters, PAG, and silicones/PFPEs.

Applications: Jet turbines, worm gear drives, refrigeration compressors, radiation-resistant systems.


Lubricating Mechanisms & Stribeck Curve Dynamics

Liquid lubricant behavior is governed by the Hersey number (η · N / P), where η represents dynamic viscosity, N is rotational speed, and P is normal load. Performance spans three tribological regimes defined by the Film Thickness Ratio (Λ = hmin / √(σ1² + σ2²)), where hmin is minimum film thickness and σ1, σ2 are the surface roughness values of the mating parts.

Boundary Lubrication

Λ < 1.2

High loads, low speeds, or low viscosity. Surface asperities make direct contact. Dispersed solid particles (MoS2, PTFE) physically separate metal peaks to minimize adhesive friction.

Mixed Lubrication

1.2 ≤ Λ ≤ 3

Partial fluid film supports part of the load, while boundary additive films and solid dispersions support the rest.

Hydrodynamic / EHL

Λ > 3

Contacting surfaces are fully separated by a continuous fluid film. Localized pressures (1–3 GPa) in non-conformal contacts exponentially increase oil viscosity, elasticizing the contacting metals.

Stribeck curve dynamics

ISO Viscosity Grade (ISO 3448) & Selection Guide

The ISO Viscosity Grade (ISO VG) system, defined under ISO 3448, is the globally accepted classification for industrial liquid lubricants, based on kinematic viscosity measured at 40°C (104°F), expressed in centistokes (cSt) or mm²/s.

Viscosity must be matched to the rotational speed of the bearing. Higher speeds require lower viscosities to prevent excessive fluid friction (viscous drag) and overheating. The DN factor is used to calculate this:

DN Speed Factor = dm × N

Where dm = (bore diameter + outer diameter) / 2 (mm), and N = rotational speed (RPM).

DN > 500,000 (High Speed)

Requires ISO VG 10 to 32

DN 100,000–500,000 (Medium Speed)

Requires ISO VG 46 to 150

DN < 100,000 (Low Speed)

Requires ISO VG 220 to 680

Higher loads compress the oil film. If viscosity is too low, the elastohydrodynamic (EHL) film collapses, leading to boundary contact. Lighter loads favor lower viscosity (ISO VG 32–68) for better cooling and lower energy use, while heavy or shock loads favor higher viscosity (ISO VG 320–680) for a thicker, more resilient fluid film.

ISO Viscosity Grade Classification Table

ISO Grade Midpoint @ 40°C (cSt) Min (cSt) Max (cSt) Typical Application
ISO VG 2 2.2 1.98 2.42 Ultra-high-speed spindles (>100,000 RPM)
ISO VG 10 10.0 9.00 11.00 High-speed precision machine tool spindles
ISO VG 22 22.0 19.8 24.2 Airline lubricators, cold-climate hydraulics
ISO VG 32 32.0 28.8 35.2 Standard industrial hydraulics, air compressors
ISO VG 46 46.0 41.4 50.6 Heavy-duty mobile hydraulics, circulating systems
ISO VG 68 68.0 61.2 74.8 Slide-ways, lightly loaded gearboxes, vacuum pumps
ISO VG 100 100.0 90.0 110.0 Moderate gearboxes, large circulating oil systems
ISO VG 150 150.0 135.0 165.0 Enclosed industrial gearboxes, chain drives
ISO VG 220 220.0 198.0 242.0 Heavy-duty spur and helical gear drives
ISO VG 320 320.0 288.0 352.0 Heavy shock-load gearboxes, rolling mill drives
ISO VG 460 460.0 414.0 506.0 Low-speed/high-load gearboxes, worm drives
ISO VG 680 680.0 612.0 748.0 Heavy industrial worm gears, extreme low-speed drives
ISO VG 1000 1000.0 900.0 1100.0 Open gear compounds, heavy dragline components

ISO 3448 only dictates viscosity at 40°C. Industrial equipment rarely operates exactly at that temperature, and oil thins as it heats up. If operating between 70°C and 100°C, the oil's Viscosity Index (VI), a dimensionless number indicating how much viscosity changes with temperature, should also be checked.


Advantages & Disadvantages

Advantages Disadvantages & Limitations
  • High heat transfer and efficient cooling via fluid circulation.
  • Flows into small contacts and can be pumped, filtered, and cooled.
  • Flushes away wear debris, contaminants, and moisture.
  • Wide operating viscosity range achievable via viscosity index improvers.
  • Dispersions provide emergency dry-run survival capability under sudden fluid loss.
  • Requires physical containment, complex dynamic sealing, and housings.
  • Risk of fluid leakage leading to environmental contamination or fire hazards.
  • Solid dispersions require strict particle size control to prevent filter plugging.
  • Thermal-oxidative degradation requires periodic fluid monitoring and drain intervals.

Key Application Sectors & Machinery Components

Lubricating oils and liquid colloidal dispersions are selected for applications requiring continuous fluid flow, active thermal dissipation, hydrodynamic/elastohydrodynamic separation, and the flushing of wear debris. Adding dispersed solid micro-particles (MoS2, PTFE, graphite, h-BN) enhances performance in machinery subjected to frequent stop-start cycles, shock loads, or extreme temperature.

1. Power Transmission & Industrial Gear Systems

Enclosed Spur, Helical, and Bevel Gears: Neat synthetic oils (ISO VG 150 to 460) maintain an elastohydrodynamic (EHL) fluid film under steady-state operating conditions.

Types of gears reference chart
Steel mill drive motor

Heavy Mining & Steel Mill Drives: Colloidal MoS2 dispersions added to heavy gear oils protect gear tooth flanks against boundary welding during sudden shock loads, heavy impact forces, or low rotational speeds.

Worm Gear Drives: Synthetic polyalkylene glycol (PAG) neat oils provide a low sliding friction coefficient, reducing thermal friction generated by steel-on-bronze sliding contacts.

Worm gear drive assembly

2. High-Speed Precision Equipment & Turbines

Machine Tool Spindles & Sewing Machines: Ultra-light neat synthetic fluids (ISO VG 2, 10, or 22) provide hydrodynamic surface separation with minimal viscous shear resistance, ensuring low running temperatures and maintaining sub-micron machining tolerances.

Machine tool spindle Sewing machine mechanism
Steam and gas turbines comparison

Steam & Gas Turbines: Group II/III mineral or PAO turbine oils (ISO VG 32 or 46) require rapid water-separating capability (demulsibility), low foaming propensity, and resistance to thermal oxidation over extended service lives, often exceeding 10,000 hours.

3. Hydraulic & Fluid Power Systems

Industrial & Mobile Hydraulics: High viscosity index (HV) anti-wear hydraulic fluids transmit mechanical force while lubricating high-pressure axial piston pumps, vane pumps, and control valves operating up to 350 bar.

Cleanroom / High-Precision Servo-Hydraulics: Fine-filtered neat synthetic esters provide flame resistance (HFDU fluids) and consistent pressure transmission without valve-sticking caused by varnish or sludge formation.

Industrial and mobile hydraulics workshop

4. Extreme High-Temperature Conveyors & Processing

Ceramic kiln high-temperature processing

Ceramic Kilns, Glass Works, & Paint Curing Ovens: Synthetic polyol ester oils carrying sub-micron colloidal graphite or hexagonal boron nitride (h-BN) are fed directly to chain links and bushings operating from 200°C to over 500°C. The ester carrier wets the pin surfaces and evaporates cleanly, leaving the graphite or h-BN behind as a dry, low-friction film.

5. Metal Forming, Forging, & Break-In Operations

Machinery Running-In & Assembly: Engine oil or gear fluid blended with 3% to 5% colloidal MoS2 is applied during initial machinery commissioning, burnishing into metal micro-asperities to accelerate smooth surface bedding.

Cold Heading & Heavy Metal Stamping: Water- or oil-based colloidal suspensions of graphite or MoS2 are sprayed directly onto forging dies to reduce friction during high-deformation metal displacement.

Cold heading punches Progressive die heavy metal stamping

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers